Quote:
Originally Posted by BusterBoyBenz View Post
What's the durometer of those parts.



I can see the advantages for a low use/wear and tear track car


The part is made from delrin acetal resin with ptfe

Specifications are ATSM D6100 ATSM D6778
Tensile strength 9,000psi
Impact strength 1.00 ft-lbs./in

Shore D is about 60-65
Rockwell hardness of about 60

For reference poly bushings are rated shore A 85 or 90

Let me know if you have any more questions.

We have sold 280 kits to date no one has complained about it. Most of the customers are from Europe since there are more 4 and 5 speeds on that side of the world.