maxsmom 11-28-2006 03:12 PM

using j/b cold weld on cracked oil pan
 
How long does a cold weld j/b gel hold?????son and I quick fixed a cracked oil pan with j/b weld to be able to get it to friends shop while waiting for new oil pan.

RAYMOND485 11-28-2006 04:45 PM

Oil Pan
 
1984 300d Turbo 141,000
Replace $28.00 Oil Pan, They Warp And Leak And New Gasket Diy

mbdoc 11-28-2006 05:59 PM

I JB welded a large section 2" X 3" of cast iron engine block on a OM617 engine & it lasted 4 years before it started leaking again.

Cleaning the surface area first is the key to success!

Palangi 11-29-2006 11:38 AM

If it's just a crack, Seal All should work well. If it's really a hole, I would try the JB Weld, but don't depend on it to last a long time.


All times are GMT -4. The time now is 09:43 AM.

Powered by vBulletin® Version 3.8.7
Copyright ©2000 - 2025, vBulletin Solutions, Inc.
Search Engine Optimization by vBSEO 3.6.0
Copyright 2024 Pelican Parts, LLC - Posts may be archived for display on the Peach Parts or Pelican Parts Website