Reversing galvanic corrosion?
Is there a way to break the bond between aluminum and steel besides brute force?
__________________
You don't need a weatherman to know which way the wind blows - Robert A. Zimmerman |
#2
|
|||
|
|||
try some acids: lemon / lime juice, vinegar, toilet boil cleaner.. they get stronger.. but do you really want to mess with that?
if its in threads somewhere: numerous high heat and cooling cycles will help break the bonds. |
#3
|
|||
|
|||
Is this related to an alloy wheel that won't come off the hub?
|
#4
|
|||
|
|||
Caustic eats aluminum. I worked in an aluminum plant for 20 years and we used a 50% caustic solution to leach the alumina out of the ore. Get a bottle of caustic drain cleaner and watch the bubbles start. Caustic won't eat the steel so let it soak until the Al. is gone.
|
![]() |