using j/b cold weld on cracked oil pan

How long does a cold weld j/b gel hold?????son and I quick fixed a cracked oil pan with j/b weld to be able to get it to friends shop while waiting for new oil pan.
Reply With Quote
  #2  
Old 11-28-2006, 04:45 PM
RAYMOND485
 
Join Date: May 2005
Location: CALIF
Posts: 508
Oil Pan

1984 300d Turbo 141,000
Replace $28.00 Oil Pan, They Warp And Leak And New Gasket Diy
Reply With Quote
  #3  
Old 11-28-2006, 05:59 PM
Moderator
 
Join Date: Mar 1999
Location: Tucker, Ga USA
Posts: 12,153
I JB welded a large section 2" X 3" of cast iron engine block on a OM617 engine & it lasted 4 years before it started leaking again.

Cleaning the surface area first is the key to success!
__________________
MERCEDES Benz Master Guild Technician (6 TIMES)
ASE Master Technician
Mercedes Benz Star Technician (2 times)
44 years foreign automotive repair
27 Years M.B. Shop foreman (dealer)
MB technical information Specialist (15 years)
190E 2.3 16V ITS SCCA race car (sold)
1986 190E 2.3 16V 2.5 (sold)
Retired Moderator
Reply With Quote
  #4  
Old 11-29-2006, 11:38 AM
Palangi's Avatar
L' Résistance
 
Join Date: Dec 2000
Location: Republique de Banana
Posts: 3,495
If it's just a crack, Seal All should work well. If it's really a hole, I would try the JB Weld, but don't depend on it to last a long time.
__________________
Palangi

2004 C240 Wagon 203.261 Baby Benz
2008 ML320 CDI Highway Cruiser
2006 Toyota Prius, Saving the Planet @ 48 mpg
2000 F-150, Destroying the Planet @ 20 mpg



TRUMP .......... WHITEHOUSE
HILLARY .........JAILHOUSE
BERNIE .......... NUTHOUSE
0BAMA .......... OUTHOUSE
Reply With Quote
Reply

Bookmarks


Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is On
Trackbacks are On
Pingbacks are On
Refbacks are On




All times are GMT -4. The time now is 09:11 PM.


Powered by vBulletin® Version 3.8.7
Copyright ©2000 - 2026, vBulletin Solutions, Inc.
Search Engine Optimization by vBSEO 3.6.0
Copyright 2024 Pelican Parts, LLC - Posts may be archived for display on the Peach Parts or Pelican Parts Website -    DMCA Registered Agent Contact Page