using j/b cold weld on cracked oil pan
How long does a cold weld j/b gel hold?????son and I quick fixed a cracked oil pan with j/b weld to be able to get it to friends shop while waiting for new oil pan.
|
#2
|
|||
|
|||
Oil Pan
1984 300d Turbo 141,000
Replace $28.00 Oil Pan, They Warp And Leak And New Gasket Diy |
#3
|
|||
|
|||
I JB welded a large section 2" X 3" of cast iron engine block on a OM617 engine & it lasted 4 years before it started leaking again.
Cleaning the surface area first is the key to success!
__________________
MERCEDES Benz Master Guild Technician (6 TIMES) ASE Master Technician Mercedes Benz Star Technician (2 times) 44 years foreign automotive repair 27 Years M.B. Shop foreman (dealer) MB technical information Specialist (15 years) 190E 2.3 16V ITS SCCA race car (sold) 1986 190E 2.3 16V 2.5 (sold) Retired Moderator |
#4
|
||||
|
||||
If it's just a crack, Seal All should work well. If it's really a hole, I would try the JB Weld, but don't depend on it to last a long time.